Polymer Products

Polymer particle

Toraymill™PPS

【SEM image】

【Particle size distribution】


【Data sheet】

Material Polyphenylene Sulfide resin
Average of particle size(μm) 15-100 ※
Form of sample Powder
Specific gravity(g/cm3) 1.34
Glass transition Temp. (℃) 85
Recrystallization Temp.(℃) 196
Melting point(℃) 285
Thermal reduction Temp.(℃) 480
Refractive index 1.7

*Specific gravity and heat property is reference value from several data.

  • ※Average of particle size adjustable to above range.

【Assumed application(Assumed)】

  • Materials for 3D printer (SLS method)
  • Additives (Improvement of heat resistance or mechanical property etc.)
  • Back
  • Print Friendly Page

* Trademarks of Toray Group in this Chemical product site are used for Japanese Customer.

TOP OF THIS PAGE

  • Terms of Use
  • Privacy Policy
  • sitemap

Toraymill™PPS

【SEM image】

【Particle size distribution】


【Data sheet】

Material Polyphenylene Sulfide resin
Average of particle size(μm) 15-100 ※
Form of sample Powder
Specific gravity(g/cm3) 1.34
Glass transition Temp. (℃) 85
Recrystallization Temp.(℃) 196
Melting point(℃) 285
Thermal reduction Temp.(℃) 480
Refractive index 1.7

*Specific gravity and heat property is reference value from several data.

  • ※Average of particle size adjustable to above range.

【Assumed application(Assumed)】

  • Materials for 3D printer (SLS method)
  • Additives (Improvement of heat resistance or mechanical property etc.)

Print